Finish defects have specific, readable causes. Orange peel comes from atomisation and viscosity, runs from over-application, dry spray from excessive distance or heat, and pinholing from contamination or trapped solvent.

Dated frames Honiton: Because each one has a distinct cause, each has a distinct remedy — and the remedy is applied at the time, not after the film has cured. Reading the surface as it goes on is a large part of the skill.
Dated frames Honiton: Because each one has a distinct cause, each has a distinct remedy — and the remedy is applied at the time, not after the film has cured. Reading the surface as it goes on is a large part of the skill.
Dated frames Honiton: Inspection is done in raking light rather than straight on. Held at a low angle, a surface reveals texture that is completely invisible from directly in front of it.
Dated frames Honiton: Inspection is done in raking light rather than straight on. Held at a low angle, a surface reveals texture that is completely invisible from directly in front of it.

surface defects decision path for Dated frames in Honiton

Because each one has a distinct cause, each has a distinct remedy — and the remedy is applied at the time, not after the film has cured. Reading the surface as it goes on is a large part of the skill.

Surface defects and what causes them in Honiton

Finish defects have specific, readable causes. Orange peel comes from atomisation and viscosity, runs from over-application, dry spray from excessive distance or heat, and pinholing from contamination or trapped solvent.

Because each one has a distinct cause, each has a distinct remedy — and the remedy is applied at the time, not after the film has cured. Reading the surface as it goes on is a large part of the skill.

Inspection is done in raking light rather than straight on. Held at a low angle, a surface reveals texture that is completely invisible from directly in front of it.

Dated frames Honiton: surface defects

Inspection is done in raking light rather than straight on. Held at a low angle, a surface reveals texture that is completely invisible from directly in front of it.

Dated frames Honiton: surface defects

In raking light at a low angle, which reveals texture a straight-on look hides. Defects are read and corrected during application rather than afterwards.

Dated frames Honiton: surface defects

Dated frames in Honiton: How do you check the quality of the finish? — what matters for Georgian High Street townhouses?
In raking light at a low angle, which reveals texture a straight-on look hides. Defects are read and corrected during application rather than afterwards.

Ready to start your project?

Free quotes · 10-year guarantee · Friendly local service.

Call now WhatsApp